dc.contributor.authorBadejo, S.O.-
dc.contributor.authorOmole, A. O.-
dc.contributor.authorFuwape, J. A.-
dc.contributor.authorOyeleye, B. O.-
dc.date.accessioned2018-10-09T10:53:37Z-
dc.date.available2018-10-09T10:53:37Z-
dc.date.issued2012-
dc.identifier.issn0331-0787-
dc.identifier.otherNigerian Journal of Agriculture, Food and Environment 7(4), pp. 111-120-
dc.identifier.otherui_art_badejo_static_2011-
dc.identifier.urihttp://ir.library.ui.edu.ng/handle/123456789/1378-
dc.description.abstractA study was carried out to determine the optima level of percent additive concentration for wood cement board production from mixed tropical hardwoods species. Eight hardwood species used for the study are: Triplochiton scleroxylon K. Schum (Obeche). Terminalia ivorensis A. Chev. (Idigbo) Terminalia superb Eng. & Diets (Afara) Bruchystegia nigerica Hoyle & A.P.D. Jones (Okwen) Khaya ivorensis A. Chev. (Lagos Mahogany) Nesogordonia papaverifeni A. Chev. (Dantu-Oro) Tectona grandis Linn. F. (Teak) Gmelina arborea Roxb. (Gmelina). The experimental boards were made at five chemical additive content levels of 1.00%: 1.50%: 2.00%: 2.50% and 3.00% based on dry weight of cement in board, and three cement/wood mixing ratio levels of 2.25: 1.0. 2.50: 1.0 and 2.75:1.0. The experimental design is a two-factor factorial experiment, a combination of which manifested in 15 treatment combinations. The mean moduli of Rupture and Elasticity (MOR and MOE) obtained for each of the 15 treatment combinations in this experiment ranged from 3.28 to 10.46 N/mm2 while MOE values ranged from 2200 to 4010 N/mm2. The mean percent water absorption (WA) values ranged from 24.66 to 46.37% while the thickness swelling (TS) ranged from 0.98 to 3.62%. Statistical analysis showed chemical additive concentration and wood/cement ratio were found significant at 1% level of probability on the flexural and moisture properties. Stronger, stiffer and more dimensionally stable boards were produced at increasing levels of these two production variables. Also percent chemical additive content in board of 3.0% (Based on dry cement weight in board) performed best.en_US
dc.language.isoen_USen_US
dc.publisherFaculty of Agriculture, University of Uyo, Nigeriaen_US
dc.subjectStatic bending,en_US
dc.subjectmoisture response,en_US
dc.subjectchemical additive,en_US
dc.subjectcement bondedparticle board additive concentrationen_US
dc.titleStatic bending and moisture response of cement-bonded particleboard produced at different levels of percent chemical additive content in boarden_US
dc.typeArticleen_US
Appears in Collections:scholarly works

Files in This Item:
File Description SizeFormat 
(28) ui_art_badejo_static_2011.pdf2.57 MBAdobe PDFThumbnail
View/Open


Items in UISpace are protected by copyright, with all rights reserved, unless otherwise indicated.